dc.identifier.citation | Laser beam welding of a Ti-15mo/TIB metal-matrix composite / M. Ozerov [et al.] // Metals. - 2021. - Vol.11, №3.-Art. 506. - Doi: 10.3390/met11030506. | ru |
dc.identifier.uri | http://dspace.bsu.edu.ru/handle/123456789/44318 | - |
dc.description.abstract | A Ti-15Mo/TiB metal-matrix composite was produced by spark plasma sintering at 1400 °C. The fractions of the elements in the initial powder mixture were 80.75 wt.% Ti, 14.25 wt.% Mo, and 5 wt.% TiB2. The initial structure of the synthesized composite was composed of bcc titanium matrix and needle-like TiB reinforcements with an average thickness of 500 ∓ 300 nm | ru |
dc.language.iso | en | ru |
dc.subject | technique | ru |
dc.subject | metal science | ru |
dc.subject | titanium-matrix composites | ru |
dc.subject | laser beam welding | ru |
dc.subject | microstructure | ru |
dc.subject | pre-heating temperature | ru |
dc.subject | TiB bunches | ru |
dc.subject | microhardness | ru |
dc.title | Laser beam welding of a Ti-15mo/TIB metal-matrix composite | ru |